Corson Alloys
Corson Alloy NKC1816
NKC1816 High Performance Corson Alloy
Overview
NKC1816 is a Corson alloy balancing strength and conductivity at higher levels than the standard C7025 Corson alloy.
Table 1. NKC1816 chemical composition (%)
Cu | Ni | Co | Si | Cr | |
---|---|---|---|---|---|
Standard composition | Remainder | 1.8 | 1.0 | 0.6 | 0.15 |
Table 2. Physical properties of NKC1816
Electrical conductivity | 47 | %IACS (@20℃) |
---|---|---|
Specific resistance | 37 | nΩ·m (@20℃) |
Thermal conductivity | 198 | W/mK |
Modulus of elasticity | 125 | GPa |
Density | 8.72 | g/cm3 |
Table 3. Mechanical properties of NKC1816
(upper: typical values, lower: specification range)
Temper | Tensile strength (MPa) |
Yield strength (MPa) |
Elongation (%) |
Vickers hardness (Hv) |
---|---|---|---|---|
ESH | 880 (840-940) |
850 (810-910) |
2 (min.1) |
270 (230-300) |